Assurance In Action: Episode 44 Testing
2026-11-01Assurance In Action: Episode 44 Testing explains how laboratories convert food and agricultural samples into defensible safety results. It follows the chain from representative sampling through screening by ELISA and lateral flow, pathogen identifica
Flow Accelerated Corrosion in Nuclear Power Plants Testing
2026-11-01Flow accelerated corrosion testing combines laboratory loop exposure of representative carbon steel coupons with in-plant ultrasonic wall thickness surveys. Controlled velocity, temperature, and water chemistry reproduce the service mechanism. Thickn
Chemical Analysis for Flexible Packaging Testing
2026-10-31Chemical analysis for flexible packaging testing quantifies residual solvents by headspace GC-MS, plasticizers and adhesive residues by HPLC, and heavy metal migration by ICP-MS, with gravimetric overall migration completing the panel. Results are no
Assurance In Action: Episode 43 Testing
2026-10-31Episode 43 of Assurance In Action describes an integrated food safety assurance workflow: representative sampling with custody control, ELISA screening of chemical hazards, HPLC confirmation of presumptive positives, and PCR detection of microbial an
Addressing the Safety of Energy Storage Systems Testing
2026-10-31Energy storage system safety testing verifies thermal runaway propagation, electrical insulation and protection functions, environmental endurance, and vented gas composition through FTIR and GC-MS analysis. Samples are prepared at defined state of c
Understanding Foreign Materials in Foods – Part 4 Testing
2026-10-31Foreign material testing in foods combines inline screening with laboratory confirmation. Metal detection and X-ray inspection locate dense contaminants such as metal, glass, and bone, while microscopy, FTIR spectroscopy, and PCR identify isolated pa
Understanding Foreign Materials in Foods – Part 3 Testing
2026-10-31Foreign material testing in foods locates and identifies physical contaminants such as metal, glass, plastic, rubber, fibers, and insect fragments. Screening uses stereomicroscopy, X-ray imaging, and metal detection; identification uses FTIR, SEM-EDS
Smart Grid Solutions and Modernization Testing
2026-10-31Smart Grid Solutions and Modernization Testing verifies intelligent electronic devices, communication networks, and control systems through protocol conformance, IEC 61850 functional testing, communication performance measurement, and structured cybe
A Day in the Life: Harry Tregartha Testing
2026-10-31This article uses a working day of laboratory engineer Harry Tregartha to explain routine testing in practice: analytical principles (chromatography, MS, spectrophotometry, ELISA, PCR), sample collection and custody, the batch workflow with calibrati
Keys to a Successful Building Mock-Up Testing
2026-10-31Successful building mock-up testing depends on a written test plan, a full-scale specimen replicating actual construction details, calibrated instrumentation for air, water, structural, and displacement testing, and pre-agreed pass-fail criteria. Seq
Removal of non-industrial chemicals from the NICNAS
2026-10-31Removal of non-industrial chemicals from NICNAS/AICIS scope is demonstrated through a testing dossier: identity confirmation by GC-MS and LC-MS, validated quantification of the declared component, impurity and residual-solvent profiling, and complian
Understanding Foreign Materials in Foods – Part 2 Testing
2026-10-31This article explains the laboratory workflow for testing foreign materials in foods: proper sample collection and preservation, physical detection by microscopy and X-ray methods, chemical identification with GC-MS and ICP-MS, and biological screeni
Understanding Foreign Materials in Foods – Part 1 Testing
2026-10-30Foreign materials in foods—metals, glass, plastics, rubber, stones, and bone fragments—are tested through a defined sequence: classification, careful sample collection, physical detection by microscopy, X-ray inspection, and metal detection, followed
A Day in the Life: Stephen Fagg Testing
2026-10-30Stephen Fagg testing describes the disciplined daily routine of a laboratory analyst: verifying assay principles and mechanisms, receiving and registering samples under chain of custody, running methods such as HPLC, GC-MS, spectrophotometry, ELISA,
Why Did My Part Break? Testing
2026-10-30Fracture failure analysis reconstructs why a part broke through a fixed sequence: secure and section the failed sample, read the fracture surface by stereomicroscopy and SEM, verify microstructure by metallography, confirm mechanical properties by te
FIPS: Is it Chaos or New CMVP Entropy Requirements? Testing
2026-10-30CMVP entropy requirements testing validates the noise source, health tests, and conditioning of an entropy source against the estimator suite in NIST SP 800-90B. Datasets of one million samples per operating condition are analyzed with most-common-va
The Challenges and Changes of IEC 61010 Testing
2026-10-30IEC 61010 testing verifies that measurement, control, and laboratory equipment withstands dielectric stress, limits leakage current, and maintains protective-earth continuity. This article explains the working principles of each test item, scope sele
Implementing an Anti-Bribery Policy in Your Management
2026-10-30Implementing an anti-bribery policy in your management means converting a written commitment into a testable system: defined scope, policy components, ranked risk assessment, third-party due diligence, clause-based gap analysis, KPI monitoring, and c
Testing and Certification in North America
2026-10-30Testing and certification in North America cover electrical, electronic, mechanical, and energy products under a mix of mandatory regulations and voluntary schemes. Evaluation relies on ASTM, ANSI, UL, and CSA standards, applied by accredited laborat
Smart Audits Testing
2026-10-30Smart Audits Testing evaluates smart and connected products through a structured chain: scope definition, checklist-based workflow, on-site sampling with documented evidence, and laboratory verification using methods such as GC-MS, HPLC, spectrophoto
FIPS: Legacy Mix-Up Testing
2026-10-30FIPS legacy mix-up testing locates residual DES, 3DES, short-key RSA, and SHA-1 usage in software, firmware, and hardware modules. Samples are collected under chain-of-custody, analyzed by paired static and dynamic methods, and scored by per-family d
Total Sustainability in Progress: Episode 14 Testing
2026-10-30Episode 14 sustainability testing evaluates materials, products and process outputs against declared sustainability criteria. It covers sample collection, GC-MS and HPLC determination, spectrophotometric endpoints, PCR identity panels, and assay perf
Understanding Standards: An Overview - Part 2 Testing
2026-10-29Standard-based testing applies published procedures to measure properties of materials, components, and assemblies against stated acceptance criteria. This overview explains the categories of standards, sample and conditioning requirements, prescribe
UPDATE – The Government of Canada’s Approach to Promote
2026-10-29Testing supporting the Government of Canada's chemical safety approach covers parent compounds, transformation products, and fate-related properties in environmental, biological, and product matrices. Determination relies on GC-MS and LC-MS/MS after
Testing and Certifying Hazardous Location Assemblies
2026-10-29Testing and certifying hazardous location assemblies verifies that enclosures and their installed components will not ignite surrounding gas or dust atmospheres. The program covers scope definition under explosion-protection standards, sample prepara
Send Us a Message
Fill out the form below and we'll respond within 24 hours.
Our Locations
Business Hours
ISO 17025 Accredited
All testing performed under rigorous quality management.