12 Instruments Available
226

Limestone and Dolomite Testing

2026-10-15

Limestone and dolomite testing combines chemical analysis (XRF, EDTA titration, loss-on-ignition), mineral phase identification by XRD, and physical tests such as particle size, density, and reactivity. After representative sampling and grinding, res

→
227

Thermal and Visual Comfort Performance Testing of Building Shading

2026-10-15

Thermal and visual comfort testing of building shading measures solar and visible transmittance and reflectance by UV–Vis–NIR spectrophotometry with an integrating sphere, derives g-value and shading coefficient through hot-box or validated simulatio

→
228

Yellow River Silt Porous Brick Testing

2026-10-13

Yellow River silt porous brick testing covers sampling by batch, drying and specimen conditioning, dimensional and appearance checks, density measurement, compression strength with shape-factor correction, boiled water absorption, and cyclic freeze-t

→
229

T-Type Door Testing for Buildings

2026-10-13

T-Type Door Testing for Buildings evaluates complete lift-and-slide and T-profile doorsets for air permeability (EN 1026 / ASTM E283), watertness (EN 1027 / ASTM E331), wind load resistance with deformation, cycling and safety stages (EN 12211 / ASTM

→
230

Fiber Bragg Grating Temperature Sensor Testing for Civil Engineering

2026-10-13

FBG temperature sensor testing for civil engineering verifies wavelength-temperature behavior before field deployment. The procedure covers specimen inspection, calibration in a thermostatic bath against a traceable reference thermometer, multi-point

→
231

Finish-Free Door Testing

2026-10-13

Finish-free door testing inspects unfinished door leaves before coating, covering surface condition, flatness and warp, dimensional accuracy, and hardware preparation fit. Measurement uses straightedges, feeler gauges, calipers, templates, and calibr

→
232

Reflective Surface Profile and Reflectance Testing of Optical Components

2026-10-13

Reflective surface profile and reflectance testing characterizes the microgeometry and photometric performance of reflective optical components. The workflow covers sample cleaning, profile measurement by stylus, white-light interferometric, or confo

→
233

Battery Failure Analysis Testing

2026-10-08

Battery failure analysis testing combines non-destructive CT imaging, SEM/EDS microscopy, impedance and capacity characterization, and chemical analysis (GC-MS, ICP-OES, XRD) to trace cell faults to their root cause. Teardown under inert atmosphere p

→
234

Quality & Performance Testing for Wireless Products

2026-10-08

Wireless product testing verifies RF performance, protocol conformance, reliability, and safety through conducted and radiated measurements, interoperability pairing, and environmental stress with re-measurement. Acceptance relies on standard limit t

→
235

ISO/IEC 20071-31:2026 – Information technology

2026-10-08

ISO/IEC 20071-31:2026 specifies requirements and recommendations for accessible kiosk design, manufacture, installation and operation. Published on 2026-08-18 by ISO/IEC JTC 1/SC 35, it addresses information presentation and user interaction across k

→
236

IEC TS 61641:2026 – Low-voltage switchgear and controlgear assemblies

2026-10-08

IEC TS 61641:2026 specifies verification methods for internal arc-fault protection of low-voltage switchgear and controlgear assemblies under the IEC 61439 series. It covers passive, active (IAMS-based), and arc ignition protected zone approaches, ad

→
237

IEC 60947-5-3:2026 – Low-voltage switchgear and controlgear

2026-10-08

IEC 60947-5-3:2026 specifies fault performance requirements for proximity devices with defined behaviour under fault conditions (PDDB) as control circuit devices and switching elements. Published 2026-08-19 by TC 121/SC 121A, it supplements IEC 60947

→
238

ISO/IEC 38505-1:2026 – Information technology

2026-10-08

ISO/IEC 38505-1:2026, published 2026-08-20 by ISO/IEC JTC 1/SC 40, applies the governance principles and model of ISO/IEC 38500 to the governance of data. It guides governing bodies of all organizations, public or private, on effective, efficient and

→
239

ISO/IEC TS 38501-2:2026 – Information technology

2026-10-08

ISO/IEC TS 38501-2:2026 is a current technical specification from ISO/IEC JTC 1/SC 40 giving guidance on the assessment scheme for implementing governance of IT in line with ISO/IEC 38500 and ISO/IEC 38501-1. It defines an assessment framework, a rat

→
240

IEC PAS 61850-90-19:2026 – Communication networks and systems for power utility automation

2026-10-07

IEC PAS 61850-90-19:2026 applies the Role-Based Access Control requirements of IEC 62351-8 to the IEC 61850 environment. It covers RBAC modelling, impacts on IEC 61850 models and protocols, engineering process requirements, and binding of permissions

→
241

IEC 63387-1:2026 – Hybrid CPV/PV modules: General characteristics and measurement procedures

2026-10-07

IEC 63387-1:2026 specifies power-rating methods for hybrid CPV/PV modules combining concentrated-light and diffuse/global-light cell arrays. It defines standard conditions, procedures for measuring power versus AOI, irradiance and temperature, a FoV

→
242

IEC 61851-23-3:2026 – Electric vehicle conductive charging system

2026-10-07

IEC 61851-23-3:2026 specifies DC EV supply equipment for megawatt charging systems, rated up to 1 000 V AC or 1 500 V DC on the supply side and 1 250 V DC on the vehicle side, using a coupler per IEC TS 63379 with protective separation. Communication

→
243

IEC 60623:2026 CMV – Secondary cells and batteries containing alkaline or other non-acid electrolyte

2026-10-07

IEC 60623:2026 CMV specifies marking, designation, dimensions, tests and requirements for vented nickel-cadmium prismatic secondary single cells and battery systems for industrial applications. The commented version pairs the sixth edition with track

→
244

ISO/IEC/IEEE 8802-A:2026 – Information technology

2026-10-07

ISO/IEC/IEEE 8802-A:2026 (published 2026-08-24, current) is the overview and architecture part for local and metropolitan area networks. It describes IEEE 802 standards for frame-based data networks, defines a reference model for protocol standards,

→
245

ISO/IEC/IEEE 8802-3:2026 – Telecommunications and exchange between information technology systems

2026-10-06

ISO/IEC/IEEE 8802-3:2026, published 2026-08-24 by ISO/IEC JTC 1/SC 6, defines Ethernet local, access and metropolitan area networks at selected speeds. It specifies the CSMA/CD MAC protocol in half and full duplex, speed specific MIIs, PHY encoding a

→
246

IEC TS 63092-3:2026 – Photovoltaics in buildings

2026-10-06

IEC TS 63092-3:2026 specifies a versatile method for determining the solar heat gain coefficient (g value) of building-integrated photovoltaic modules. It uses calorimetric hot box or cooled plate methods per ISO 19467, accounts for electricity extra

→
247

ISO/IEC 21617-1:2026 – Information technology - JPEG Trust - Part 1: Core foundation

2026-10-06

ISO/IEC 21617-1:2026 specifies a framework for establishing trust in media, covering authenticity, provenance, attribution, intellectual property rights and integrity through secure, reliable annotation of media assets across their life cycle. Publis

→
248

IEC 63287-4:2026 – Semiconductor devices

2026-10-06

IEC 63287-4:2026 gives guidelines for developing reliability qualification plans for semiconductor devices using early failure assessment, based on environmental conditioning and proposed product usage. Published 2026-08-28 by IEC TC 47, it excludes

→
249

ISO/IEC 29128-2:2026 – Information security, cybersecurity and privacy protection

2026-10-06

ISO/IEC 29128-2:2026 specifies evaluation methods and activities for cryptographic protocols, extending the ISO/IEC 15408-4 framework. It maps evaluation work items to concrete activities and methods, and defines four increasing assurance levels base

→
250

IEC 60728-114:2026 – <p>Cable networks for television signals, sound signals and interactive s

2026-10-05

IEC 60728-114:2026 specifies system and equipment parameters and methods of measurement for FTTH/FTTB cable networks using RF over glass (RFoG) technology. It covers systems composed of an R-ONU, an xPON-based optical distribution network and an RFoG

→
 514   首页 上一页 8 9 10 11 12 13 14 15 16 17 下一页 尾页