Plastic Charpy impact testing measures the energy a notched specimen absorbs when a pendulum fractures it under three-point bending. The absorbed energy, divided by the notch cross-section, gives impact strength in kJ/m². The method is standardized in ISO 179 and ASTM D6110 and is widely used for material screening, quality control, and specification compliance.

Plastic

Charpy impact testing: principle & instrumentation
The test rests on energy conservation. A pendulum hammer of defined mass is released from a raised position. It strikes a notched specimen supported horizontally on two anvils. The fracture absorbs part of the pendulum's stored potential energy. The residual energy carries the hammer to a reduced height on the opposite side. The difference between initial and post-impact readings, after friction correction, is the absorbed impact energy. A Charpy apparatus consists of a rigid frame, a pendulum with interchangeable hammers of different energy capacities, support anvils with fixed span, a striker (striking edge), and a graduated energy scale or electronic encoder. Modern instruments add automatic energy acquisition, pneumatic or motorized release, and temperature chambers for conditioned testing. The striker radius and support geometry must match the selected standard. Both directly influence the stress state at the notch root.

Sample preparation and notch machining

Specimens are typically rectangular bars molded or machined from the material under evaluation. Dimensions and tolerances follow the governing standard. The specimen length is oriented so the notch lies at midspan and perpendicular to the striking direction. Notch quality dominates the result: the notch concentrates stress and defines the stressed volume at the crack tip. Notches are produced with a single-tooth milling cutter, a shaping tool, or a dedicated notching machine. The cutter profile must match the required notch type (A, B, or C geometries, which differ in tip radius and depth). Machining must avoid heating, smearing, or residual stresses at the notch root; all of these distort the measured energy. Cutters are inspected for wear and radius accuracy at regular intervals. After notching, specimens are conditioned at defined temperature and humidity, usually 23 °C and 50 % relative humidity, for the period stated in the specification. This brings the material to a reproducible moisture and thermal equilibrium.

Test procedure and parameter settings

Operation begins with hammer selection. The absorbed energy should fall within the readable range of the pendulum, commonly between about 10 % and 80 % of capacity. The loss must be large enough to resolve yet insufficient to stall the hammer. The operator verifies the span between anvils, aligns the specimen with the notch facing the striker, and confirms zero after a free-swing check. An air or blank swing establishes the friction correction. After release, the specimen fractures and the instrument records absorbed energy, either read from the scale or captured electronically. Key parameters include hammer energy, striker radius, support span, notch type, and test temperature. Testing at sub-ambient or elevated temperatures requires a conditioning cabinet and a defined transfer time from cabinet to anvils, typically limited to seconds so the specimen temperature does not drift. Complete break, partial break, and non-break outcomes are all recorded. Non-break results carry specific meaning in data evaluation.

Impact

strength calculation & data evaluation
The primary result is absorbed impact energy, expressed in joules. Dividing this energy by the cross-sectional area of the specimen at the notch yields Charpy impact strength, in kJ/m². This is the value most specifications cite. Notched results quantify notch sensitivity and crack-initiation resistance. Unnotched results, run on plain bars under the same geometry, reflect the energy to initiate as well as propagate fracture. Evaluation requires at least the minimum number of replicate specimens defined by the standard, since plastics scatter noticeably in impact data. Each specimen's fracture mode is recorded as complete break, hinge break, partial break, or non-break. Means computed from mixed populations are treated with caution. Partial or non-break values are reported as such rather than averaged. When specimens do not break, some laboratories report the energy as exceeding the hammer capacity or compute a notional strength with a footnote. Statistics normally reported include individual values, mean, and standard deviation.

Applicable

standards and acceptance criteria
The principal methods are the ISO 179 series for Charpy impact on plastics and ASTM D6110 for plastics in the Charpy mode. Related ASTM methods for Izod impact, such as D256, use a different specimen support but appear in many specifications alongside Charpy. ISO 179 covers instrumented variants that record force–displacement traces, distinguishing initiation from propagation energy. Acceptance criteria are not fixed by the test method itself. They are set by product standards, material datasheets, or contract between purchaser and supplier. The limit is typically a minimum mean impact strength in kJ/m² at a stated temperature and notch type. Compliance evaluation must verify specimen geometry, conditioning history, hammer capacity, and fracture-mode distribution before comparing a result with the limit. Results below the limit may reflect material degradation, poor notching practice, or a mismatched test temperature. Retesting is warranted whenever the record shows such anomalies. Accredited laboratories report full test conditions alongside the numerical result.

Applications across materials

Charpy testing applies across the breadth of thermoplastics and thermosets. Materials range from commodity polyolefins such as polyethylene and polypropylene to engineering resins such as polyamide, polycarbonate, ABS, and PVC compounds, as well as filled, glass-reinforced, and fiber-composite formulations. Impact data guide toughener and filler development, batch release in production, and grade selection for parts exposed to shock loading or cold service. The test complements other plastic evaluations covered in related resources. For example, Foam plastic testing, plastic film testing, and drop ball impact testing address forms where pendulum methods fit poorly, while aluminum Charpy impact testing follows a parallel principle in metallic materials. Charpy results at multiple temperatures map the ductile-to-brittle transition that governs low-temperature fitness of many thermoplastics. Designers use these data comparatively, ranking candidate materials rather than treating the value as a design allowable.

Quick Answers

Frequently Asked Questions

01

What

determines whether a specimen passes or fails a Charpy impact test?
Pass or fail is judged against an acceptance limit set by a product standard, material datasheet, or contractual specification. The limit is expressed as a minimum impact strength in kJ/m² at a stated temperature and notch type. The test method itself does not set a universal limit. Valid judgment also requires confirming specimen geometry, conditioning, hammer capacity, and the distribution of fracture modes before comparing the result with the limit.

02

Which

plastics and products are within the scope of Charpy impact testing?
The method covers most rigid and semi-rigid plastics, including polyolefins, polyamide, polycarbonate, ABS, PVC compounds, thermosets, and filled or reinforced grades. It suits molded or machined bar specimens. Flexible films, foams, and soft elastomers are generally evaluated with other procedures such as film, foam, or drop ball impact testing rather than pendulum Charpy.

03

What

information does a Charpy impact report contain?
A typical report states the test method, specimen dimensions and notch type, conditioning and test temperature, hammer capacity, individual absorbed energies and fracture modes, the calculated mean impact strength in kJ/m² with standard deviation, and the identification of the material and sampling basis. The report can be used for internal quality control, grade comparison, and specification compliance against agreed limits.

← Previous Article Seat belt testing
Next Article → Security door testing

Ready to Discuss Your Testing Needs?

Contact our team for a customized quote and expert consultation on your plastic Charpy impact testing testing requirements.

Contact Our Team
n n n n n n n n n n