# Titanium Salt Spray corrosion testing

Titanium salt spray corrosion testing measures how well titanium and its alloys resist corrosion. Specimens sit in a chamber filled with a controlled salt mist. The test checks coating integrity, anodized layers, conversion films, and welded or creviced areas where local breakdown may occur. It covers specimen preparation, the three main methods (NSS, ASS, CASS), evaluation metrics, acceptance criteria, and typical applications.

Titanium

salt spray corrosion testing — principle & purpose
The test speeds up chloride-induced corrosion. A sodium chloride solution is atomized into a fine mist that settles continuously on specimens held at elevated temperature. Droplets keep a thin electrolyte film on the surface. In this film, chloride ions attack the passive TiO2 layer. This reveals weak points such as pinholes in coatings, weld heat-affected zones, or crevice locations. Unlike natural atmospheric exposure, the chamber holds temperature, salt concentration, solution pH and collection rate within narrow limits. Results are therefore reproducible and comparative, not a direct prediction of service life. The purpose is threefold. First, screen surface treatments and coating systems. Second, compare batch-to-batch consistency. Third, confirm that processing steps such as pickling, anodizing or thermal oxide removal have not degraded corrosion performance. The test complements the general Salt spray test framework and broader titanium alloy testing programs.

Sample

preparation and specimen requirements
Specimens should represent the production surface. Use the same alloy grade, heat treatment condition, surface finish and coating process as the parts being qualified. Recommended dimensions let several assessment faces fit on the rack at the specified 15 to 30 degree inclination. Protect sharp edges and identification marks with inert masking tape or wax. Before exposure, clean surfaces with solvents or lint-free wipes. Avoid abrasives that alter roughness or remove oxide films. Record mass to analytical balance precision when gravimetric corrosion rate will be measured. Post-test mass loss calculation depends on the initial value. Do not passivate, degrease with harsh alkalis, or handle bare surfaces with bare fingers after cleaning. For coated specimens, mark the coating type and thickness. Keep at least one unexposed reference specimen for appearance comparison during rating.

Test

methods — NSS, ASS and CASS exposure
Three chamber methods differ in solution chemistry and severity. Neutral salt spray (NSS) uses a 5 percent sodium chloride solution at pH 6.5 to 7.2 and 35 °C. It is the baseline method for passive metals, anodized titanium and organic coatings. Acetic acid salt spray (ASS) acidifies the same solution to pH 3.1 to 3.2. It is more aggressive and suits decorative plating and detection of under-film corrosion on titanium components with metallic overlays. Copper-accelerated salt spray (CASS) adds copper chloride dihydrate to the acidified solution. It typically runs at 49 to 50 °C and applies to more severe qualification of plated or anodized finishes. In all three methods, daily verification of fog collection rate, collected solution density and pH is mandatory. Exposure duration is set by the product specification or the applicable acceptance standard. Runs of graded severity may be used to bracket performance.

Evaluation

metrics — corrosion rate and rating
Two families of metrics are reported. Gravimetric corrosion rate comes from mass loss after chemical removal of corrosion products in a cleaning solution specified for titanium. It is calculated per unit area and time, expressed as mass loss per area per time unit or converted to penetration depth per year. Appearance-based rating counts corrosion defects. Rating numbers describe the occurrence and spread of rust or corrosion products, assessed against photographic standards or by counting defects within defined areas. For coated specimens, record blister size and density, scribe-line undercut distance after cross-cut scribing, and adhesion retention. Evaluate immediately after exposure and again after drying. Some defects become visible only after 24 hours. Report the number of specimens assessed, individual ratings and the mean. Photograph representative surfaces for traceability.

Acceptance

criteria and reference standards
Acceptance is defined by the product or purchase specification, not by the test method itself. Typical criteria specify the maximum exposure duration with no corrosion products on significant surfaces, a minimum rating number, or a maximum scribe undercut width. The governing framework standards include the ISO 9227 series, which specifies the apparatus and operating conditions for NSS, ASS and CASS; ISO 4628 for evaluation of degradation of coatings; and ASTM B117 and ASTM B368 for neutral and copper-accelerated exposure respectively. Sector specifications layer additional requirements onto these base methods, such as longer durations or zero-defect limits for aerospace fasteners. A test report should state the method, chamber parameters, verification records, exposure duration and evaluation results. This lets acceptance be judged against the cited criterion without ambiguity.

Application scenarios for components

Salt spray qualification is routinely applied to titanium components where a surface treatment or joining process could compromise the native passive film. Examples include anodized titanium fasteners and aerospace structural hardware. It also covers chemically or thermally oxidized medical implant surfaces prior to coating, titanium heat-exchanger tubing with welded joints, and painted or metalized titanium panels in marine and offshore equipment. The test also serves quality control for plating on titanium substrates. CASS exposure reveals porosity and under-film attack faster than neutral spray. Compared with immersion or electrochemical techniques, chamber exposure reproduces the cyclic wet film characteristic of marine atmospheres. It also permits many specimens in one run. Buyers use the resulting report for incoming inspection, supplier qualification and batch release decisions in chloride-bearing service environments.

Quick Answers

Frequently Asked Questions

01

How are titanium salt spray corrosion test results judged, and what limits are referenced?

Judgment relies on the evaluation metrics defined in the test plan, such as corrosion rate and appearance rating of corrosion defects. Results are compared against acceptance criteria agreed between parties and the applicable reference standards. There is no single universal limit for titanium salt spray corrosion.

02

Which

products and materials are suitable for titanium salt spray corrosion testing?
The test applies to titanium and titanium alloy components across the application scenarios covered. These include fasteners, machined parts, coatings and surface-treated components. It is intended where marine or corrosive service environments must be simulated.

03

What

does a titanium salt spray corrosion test report typically include?
A report normally documents sample preparation and specimen details, the chosen exposure method (NSS, ASS or CASS), test conditions and duration, evaluation metrics such as corrosion rate and rating, and the conclusion against acceptance criteria and reference standards.

← Previous Article Seat belt testing
Next Article → Security door testing

Ready to Discuss Your Testing Needs?

Contact our team for a customized quote and expert consultation on your titanium salt spray corrosion testing testing requirements.

Contact Our Team
n n n n n n n n n n